▎ 摘 要
Here we present a novel approach to prepare N-doped graphene under ambient conditions by denitrifying bacteria CFMI-1. The N element can be effectively introduced into graphene and 8.2% (atom%) N doping level can be achieved. N-doped graphene possesses a size around 300-600 nm and an average thickness of 1-2 nm.