▎ 摘 要
Highly-qualified graphene was prepared by the ultrasonic exfoliation of commercial expanded graphite (EG) under the promotion of (NH4)(2)CO3 decomposition. The yield of graphene from the first exfoliation is 7 wt%, and it can be increased to more than 65 wt% by repeated exfoliations. Atomic force microscopy, x-ray photoelectron spectroscopy and Raman analysis show that the as-prepared graphene only has a few defects or oxides, and more than 95% of the graphene flakes have a thickness of similar to 1 nm. The electrochemical performance of the as-prepared graphene is comparable to reduced graphene oxide in the determination of dopamine (DA) from the mixed solution of ascorbic acid, uric acid and DA. These results show that the decomposition of (NH4)(2)CO3 molecules in the EG layers under ultrasonication promotes the exfoliation of graphite and provides a low-priced route for large scale production of highly-quality graphene.