• 专利标题:   Preparation of natural polymer material using rare earth metal ion coordination, involves dissolving carboxyl-modified graphene oxide and natural high molecular compound, molding, adding into rare earth metal salt solution and reacting.
  • 专利号:   CN106243240-A
  • 发明人:   FU G, HUANG Q, YAO F
  • 专利权人:   UNIV SOUTHEAST
  • 国际专利分类:   A61L027/02, A61L027/20, A61L027/50, C08B037/00, C08B037/04, C08J003/24, C08K003/04, C08K007/00, C08K009/04, C08L005/00, C08L005/04
  • 专利详细信息:   CN106243240-A 21 Dec 2016 C08B-037/04 201717 Pages: 11 Chinese
  • 申请详细信息:   CN106243240-A CN10613695 29 Jul 2016
  • 优先权号:   CN10613695

▎ 摘  要

NOVELTY - The preparation method of natural polymer material using rare earth metal ion coordination involves dissolving carboxyl-modified graphene oxide and natural high molecular compound in de-ionized water to prepare high-viscosity solution, loading high-viscosity solution into an open mold, adding into the rare earth metal salt solution, reacting, immersing natural polymer cross-linking network with rare earth metal ion coordination reaction in de-ionized water, and removing residual rare earth metal ions in the natural polymer cross-linking network by ion diffusion method. USE - Preparation method of natural polymer material using rare earth metal ion coordination (claimed). ADVANTAGE - The method enables preparation of natural polymer material with excellent biocompatibility, biodegradability, improved mechanical strength, and mild reaction condition, by simple and easy process. DETAILED DESCRIPTION - The preparation method of natural polymer material using rare earth metal ion coordination involves dissolving carboxyl-modified graphene oxide and natural high molecular compound in de-ionized water to prepare high-viscosity solution, loading high-viscosity solution into an open mold, adding into the rare earth metal salt solution, reacting at room temperature for 6-12 hours, immersing natural polymer cross-linking network with rare earth metal ion coordination reaction in de-ionized water, and removing residual rare earth metal ions in the natural polymer cross-linking network by ion diffusion method, where the mass ratio of carboxyl-modified graphene oxide and natural high molecular compound is x:1, and the concentration of the rare earth metal ion is 0.01-0.05 mol/l. x=0.001-0.02.