▎ 摘 要
NOVELTY - Packing container comprises antibacterial layer prepared using a composition containing 0.05-60 pts. wt. antimicrobial agent and 40-99.95 pts. wt. base resin. The antimicrobial agent comprises mesophilic calcium powder, ion exchange calcium powder, hydrophilic ceramic powder, hydrophobic powder and antimicrobial polymer. The mesophilic calcium powder is dried for 12-36 hours at 100-150 degrees C after washing the calcium agent with water. The dried calcium agent is crushed to prepare a first crushed product, heated at 150-300 degrees C for 1-6 hours, and secondary heated at 300-500 degrees C for 1-12 hours, and then, mesophilized through a mesophilic sintering method of third heating for a period of time, and the mesophilized primary crushed product is prepared by secondary crushing to make 0.5-50 microns average particle size. It contains at least one selected from the group consisting of shells and egg shells. USE - Packing container. ADVANTAGE - The packing container exhibits excellent antibacterial properties and antifungal properties, can be safely protected for a long time, applied to multiple containers such as cosmetic containers, pharmaceutical containers, food containers, beverage containers, storage containers, etc., and industrial by-products discarded such as shells, egg shells, and coffee foil, can be reused, is eco-friendly, and can be applied to a method for manufacturing a variety of plastic products.