• 专利标题:   Preparation of bismuth/graphitic carbon nitride semimetal-organic composite light catalyst by mixing precursor, graphene-type carbide and nitrogen substance, adding nitric acid solution, regulating pH, heating and in-situ depositing.
  • 专利号:   CN104607240-A
  • 发明人:   DONG F, LI P, SUN Y, ZHAO Z
  • 专利权人:   UNIV CHONGQING TECHNOLOGY BUSINESS
  • 国际专利分类:   B01J027/24, B01J031/02, B01J031/06
  • 专利详细信息:   CN104607240-A 13 May 2015 B01J-031/02 201555 Pages: 17 Chinese
  • 申请详细信息:   CN104607240-A CN10076346 12 Feb 2015
  • 优先权号:   CN10076346

▎ 摘  要

NOVELTY - Preparation of bismuth/graphitic carbon nitride (Bi/g-C3N4) semimetal-organic composite light catalyst comprises taking precursor, graphene-type carbide and nitrogen substance, mixing to obtain mixture, adding 1 ml/L nitric acid solution to obtain mixture solution, regulating pH at 1-2, heating in reducing system by reducing solvent, in-situ depositing and heating at 80-210 degrees C for 1-48 hours. USE - Method for preparing Bi/g-C3N4 semimetal-organic composite light catalyst (claimed). ADVANTAGE - The catalyst solves the problem about using expensive noble metal light catalyst. DESCRIPTION OF DRAWING(S) - The drawing shows a schematic diagram of preparation of bismuth/graphitic carbon nitride semimetal-organic composite light catalyst (Drawing includes non-English language text).