• 专利标题:   Ultraviolet coating paint comprises organosilicone modified epoxy acrylic resin, hydroxyapatite doped nano-silicon dioxide composite modified body, graphene additive, cellulose acetate butyrate, wetting agent, auxiliary agent, anti-settling agent, and deionized water.
  • 专利号:   CN115160877-A, CN115160877-B
  • 发明人:   LIU G, HAN Y, FAN X, YANG Q
  • 专利权人:   JUNZILAN COATING TIANJIN CO LTD
  • 国际专利分类:   C09D133/04, C09D007/62, C09D007/65
  • 专利详细信息:   CN115160877-A 11 Oct 2022 C09D-133/04 202200 Chinese
  • 申请详细信息:   CN115160877-A CN10960772 11 Aug 2022
  • 优先权号:   CN10960772

▎ 摘  要

NOVELTY - Ultraviolet coating paint, comprises 65-75 pts. wt. organosilicone modified epoxy acrylic resin, 15 -25 pts. wt. hydroxyapatite doped nano-silicon dioxide composite modified body, 10-15 pts. wt. graphene additive, 3-7 pts. wt. cellulose acetate butyrate, 3-7 pts. wt. wetting agent, 2-6 pts. wt. auxiliary agent, 1-5 pts. wt. anti-settling agent, and 85-100 pts. wt. deionized water. USE - Used as an ultraviolet coating paint. ADVANTAGE - The ultraviolet coating paint: has excellent light retention, color retention, not easy to pulverize, good gloss, as matrix raw material, which can optimize the gloss and mechanical properties of the product. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing ultraviolet coating paint comprising (1) taking raw materials, organosilicone modified epoxy acrylic resin, cellulose acetate butyrate and deionized water, firstly uniformly stirring to obtain solution A, (2) stirring the hydroxyapatite doped nano silicon dioxide composite modified body, graphene additive and mixing fully to obtain the additive B, and (4) adding wetting agent to the solution A, film-forming auxiliary agent, anti-settling agent and additive B, mixing uniformly to obtain the UV coating paint.