▎ 摘 要
NOVELTY - Graphene oxide modified polypropylene power cable protection tube comprises e.g. 60-80 pts. wt. polypropylene, 5-20 pts. wt. butadiene rubber, 5-10 pts. wt. acrylonitrile-butadiene-styrene copolymer, 5-10 pts. wt. metallocene polyethylene, 2-5 pts. wt. nano-silica sol, 2-10 pts. wt. graphene oxide, 3-10 pts. wt. nano calcium carbonate, 1-5 pts. wt. talc, 1-5 pts. wt. polyacrylonitrile fiber, 2-10 pts. wt. terminal carboxy liquid nitrile rubber, 2-10 pts. wt. maleimide, 0.5-1.5 pts. wt. dicumyl peroxide, 0.1-1 pts. wt. antioxidant, and 2-5 pts. wt. silane coupling agent. USE - Used as graphene oxide modified polypropylene power cable protection tube. ADVANTAGE - The tube is strong, impact resistant and corrosion resistant. DETAILED DESCRIPTION - Graphene oxide modified polypropylene power cable protection tube comprises 60-80 pts. wt. polypropylene, 5-20 pts. wt. butadiene rubber, 5-10 pts. wt. acrylonitrile-butadiene-styrene copolymer, 5-10 pts. wt. metallocene polyethylene, 2-5 pts. wt. nano-silica sol, 2-10 pts. wt. graphene oxide, 3-10 pts. wt. nano calcium carbonate, 1-5 pts. wt. talc, 1-5 pts. wt. polyacrylonitrile fiber, 2-10 pts. wt. terminal carboxy liquid nitrile rubber,1-5 pts. wt. phenolic resin, 1-5 pts. wt. polytetrafluoroethylene, 1-3.5 pts. wt. epoxidized soybean oil, 2-10 pts. wt. maleimide, 0.5-1.5 pts. wt. dicumyl peroxide, 0.1-1 pts. wt. antioxidant, 0.1-0.5 pts. wt. diethylenetriamine (3,4-dimethyl) benzyl sorbitol and 2-5 pts. wt. silane coupling agent.