▎ 摘 要
NOVELTY - A non-metallic heteroatom-doped reduced graphene oxide is prepared by formulating 0.1-5 mg/mL graphene oxide solution, adding non-metallic reducing agent at 70-120 degrees C, stirring for 3 hours, maintaining temperature at 70-120 degrees C, stirring for 18-48 hours, centrifuging, washing, and drying. USE - Method for preparing non-metallic heteroatom-doped reduced graphene oxide used as reduction catalyst (claimed).