▎ 摘 要
NOVELTY - The preparation of ceramic product involves (1) mixing 1.5-2.0 wt.% graphene oxide, 83-83.5 wt.% clay and 15 wt.% zirconium oxide, injecting into a ball mill, grinding, adding water, grinding to fineness of 300 mesh, (2) precipitating slurry, removing upper layer clear liquid, collecting precipitate, drying in sun for 40-50 days, (3) placing into refining machine, refining slurry, excluding slurry in air, (4) drying in drying chamber at 40-50 degrees C, (5) obtaining ceramic blank, calcining at 1200-2000 degrees C for 4-12 hours, and cooling naturally. USE - Preparation of graphene oxide containing ceramic product (claimed). ADVANTAGE - The method enables preparation of graphene oxide containing ceramic product improved density, tensile strength and hardness, reduced damage and accident rate.