▎ 摘 要
NOVELTY - A high air salt concentration galvanized iron art railing forging processing technique comprises heating iron rail, separating iron block impurity from the iron block by forging, immersing iron rail into the oil removing solution to remove the surface of the oil stains and ash, washing with deionized water, immersing in surfactant for 30-90 seconds, drying, soaking in the zinc plating tank for soaking type surface layer and inner layer soaking treatment at 5-10degrees Celsius, washing, drying, passing through the blowing cleaning platform, pre-heating at 60-120degrees Celsius, evaporating residual water of the workpiece, utilizing electrostatic spraying gun to spray the zinc powder spraying agent to thickness of 50-70 microm, checking spraying quality, curing, taking out, spraying with zinc powder coating agent using the electrostatic spraying gun to thickness of 80-100 microm, checking spraying quality, and curing. USE - High air salt concentration galvanized iron art railing forging processing technique. ADVANTAGE - The product has high salt air barrier and avoids rust formation.