• 专利标题:   Graphene/silicon dioxide/silicon/soft carbon laminated composite cathode material preparing method, involves cooling graphene/silicon dioxide/silicon/soft carbon laminated composite cathode material at room temperature.
  • 专利号:   CN103531754-A, CN103531754-B
  • 发明人:   CHEN X, LIAN T, LIU W, SHU J, TANG X
  • 专利权人:   NINGBO CARL NEW MATERIAL TECHNOLOGY CO
  • 国际专利分类:   H01M004/36
  • 专利详细信息:   CN103531754-A 22 Jan 2014 H01M-004/36 201421 Pages: 6 Chinese
  • 申请详细信息:   CN103531754-A CN10511234 17 Oct 2013
  • 优先权号:   CN10511234

▎ 摘  要

NOVELTY - The method involves adding graphene and ethyl orthosilicate in ethanol. The added solution is sprayed by using a spray dryer to obtain a silicon dioxide composite material. The material is soaked in copper acetate solution. The soaked material is filtered and dried for 5 minutes. Graphene/silicon dioxide/silicon/soft carbon laminated composite cathode material is cooled at room temperature. USE - Graphene/silicon dioxide/silicon/soft carbon laminated composite cathode material preparing method. ADVANTAGE - The method enables ensuring high electronic conductivity and effectively improving material electrochemical performance. DESCRIPTION OF DRAWING(S) - The drawing shows a graph illustrating a graphene/silicon dioxide/silicon/soft carbon laminated composite cathode material preparing method. '(Drawing includes non-English language text)'