▎ 摘 要
NOVELTY - The preparation method of anti-corrosion coating involves dispersing polymer in aqueous solution of organic acid monomer, adding aqueous solution of graphene oxide, stirring, ultrasonically treating, adding ammonium persulfate, continuously stirring for 6-18 hours followed by filtration, washing the filtration product with water, washing with alcohol for several times for neutralizing the cleaning solution, drying the precursor powder, mixing precursor powder, pigment, epoxy resin, curing agent and water to obtain a slurry, and stirring to obtain the suspension of anti-corrosion coating. USE - Preparation of anti-corrosion coating (claimed). ADVANTAGE - The method prepares environmentally-friendly anti-corrosion coating, and reduces the content of organic matter. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for the anti-corrosion coating.