▎ 摘 要
NOVELTY - Preparing modified nano-carbon material, comprises calcining nano-carbon material and molecular sieve-containing template agent together at 300-600degreesC for 1-12 hours to obtain final product, where the oxygen content in atmosphere is 8-20 vol %. USE - The modified nano-carbon material is useful in preparing olefins by dehydrogenating alkane (claimed). ADVANTAGE - The modified nano-carbon material: has better catalytic activity. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for modified nano-carbon material prepared by above method.