• 专利标题:   Manufacturing new energy pendant, comprises preparing basic material, adjusting proper proportion of melamine forming machine by material, manufacturing pendant mold, putting adjusted material into pendant mold for extrusion forming to obtain pendant semi-finished product.
  • 专利号:   CN115104824-A
  • 发明人:   XIA Y
  • 专利权人:   ZHEJIANG CAIFENG WANGQI TECHNOLOGY CO
  • 国际专利分类:   A44C025/00
  • 专利详细信息:   CN115104824-A 27 Sep 2022 A44C-025/00 202201 Chinese
  • 申请详细信息:   CN115104824-A CN10740467 28 Jun 2022
  • 优先权号:   CN10740467

▎ 摘  要

NOVELTY - Manufacturing new energy pendant comprises preparing basic material comprising 1000 meshes of melamine powder, magnetic stone powder, germanium stone powder, negative ion powder, pearl powder, pearl shell powder, pearl shell powder, far infrared powder, graphene powder, light powder; adjusting proper proportion of melamine forming machine by the material comprising 70 wt.% of 1000 meshes of melamine powder, 3 wt.% of 1000 meshes of magnetic stone powder, 3 wt.% of 1000 meshes of germanium powder, 3 wt.% of 1000 meshes negative ion powder, 3 wt.% of 1000 meshes of pearl powder, 3 wt.% of 1000 meshes pearl shellfish powder, 3 wt.% of 1000 meshes pearl shell powder, 3 wt.% of 1000 meshes far infrared powder, 3 wt.% of 1000 meshes graphene powder, 6 wt.% of 1000-mesh bright powder; manufacturing the pendant mold; putting the adjusted material into the pendant mold for extrusion forming to obtain the pendant semi-finished product. USE - Method for manufacturing new energy pendant. ADVANTAGE - The method solves the pendant of complex manufacturing technique, high energy consumption and not environment-friendly, so as to reach the rich components, extruding and forming by the mold, improving the production efficiency, reducing the labor intensity, energy-saving and environment- friendly. DETAILED DESCRIPTION - Manufacturing new energy pendant comprises preparing basic material comprising 1000 meshes of melamine powder, magnetic stone powder, germanium stone powder, negative ion powder, pearl powder, pearl shell powder, pearl shell powder, far infrared powder, graphene powder, light powder; adjusting proper proportion of melamine forming machine by the material comprising 70 wt.% of 1000 meshes of melamine powder, 3 wt.% of 1000 meshes of magnetic stone powder, 3 wt.% of 1000 meshes of germanium powder, 3 wt.% of 1000 meshes negative ion powder, 3 wt.% of 1000 meshes of pearl powder, 3 wt.% of 1000 meshes pearl shellfish powder, 3 wt.% of 1000 meshes pearl shell powder, 3 wt.% of 1000 meshes far infrared powder, 3 wt.% of 1000 meshes graphene powder, 6 wt.% of 1000-mesh bright powder; manufacturing the pendant mold; putting the adjusted material into the pendant mold for extrusion forming to obtain the pendant semi-finished product; putting the pendant semi-finished product into magnetizing machine to magnetize to obtain new energy pendant.