▎ 摘 要
NOVELTY - Preparing cotton textile antistatic agent comprises (i) adding 1-2 pts. wt. graphene oxide and 6-8 pts. wt. sodium azide into 10-20 pts. wt. water, stirring for 0.5-1 hour, filtering, washing, and drying to obtain sodium azide modified graphene oxide, (ii) adding 5-10 pts. wt. sodium azide modified graphene oxide and 5-10 pts. wt. powdered sodium periodate into 10-20 pts. wt. water, mixing and stirring for 0.5-1 hour, filtering, washing, and drying to obtain the modified graphene oxide, (iii) adding 5-10 pts. wt. modified graphene oxide, 5-10 pts. wt. zinc chloride solution and 20-30 pts. wt. water, mixing, using carbamide solution to adjust the pH to 8, and performing hydrothermal reaction to obtain the mixed solution, (iv) adding 1-2 pts. wt. diluted hydrochloric acid solution and 5-10 pts. wt. mixed solution, and stirring for 0.5-1 hours to obtain the antistatic agent. USE - The method is useful for preparing cotton textile antistatic agent. ADVANTAGE - The method improves the washing resistance and durability of the antistatic agent.