▎ 摘 要
NOVELTY - An anti-corrosion heat-dissipating powder paint comprises 40-60 pts. wt. epoxy resin, 15-25 pts. wt. composite iron titanium powder, 2-5 pts. wt. graphene, 2-5 pts. wt. carbon nanotube, 5-10 pts. wt. aluminum nitride, 2-8 pts. wt. tetramethylethylenediamine, and 10-15 pts. wt. curing agent. USE - Anti-corrosion heat-dissipating powder paint. ADVANTAGE - The powder paint has prolonged anti-corrosive performance, good heat-dissipating performance, and super strong dispersion. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of powder paint comprising adding dispersion machine with epoxy resin, boron nitride, aluminum nitride and curing agent, adding dispersant and anti-settling agent, dispersing for 15-30 minutes, adding composite iron titanium powder, dispersing for 5-8 minutes, adding graphene and carbon nanotube, ultrasonically dispersing at 80 W and at 30 kHz for 30 minutes, melt-extruding through double-screw extruder, cooling, tableting, grinding, sieving through 250-300 mesh sieve, and discharging.