• 专利标题:   Porous film comprises silicone rubber precursor, graphene, solvent, and non-solvent or pore-forming agent, where graphene is multi-layer graphene, single-layer graphene, graphene oxide, reduced graphene oxide, modified graphene.
  • 专利号:   CN107312188-A
  • 发明人:   XIA H, LUO G, HU X, QIAN W, WANG Y, WANG Z, FEI G
  • 专利权人:   UNIV SICHUAN
  • 国际专利分类:   A61L015/18, A61L015/26, A61L015/42, A61L015/46, A61L027/08, A61L027/18, A61L027/50, A61L027/56, A61L027/60, C08J005/18, C08J009/26, C08J009/28, C08L083/04
  • 专利详细信息:   CN107312188-A 03 Nov 2017 C08J-005/18 201783 Pages: 11 Chinese
  • 申请详细信息:   CN107312188-A CN10650653 02 Aug 2017
  • 优先权号:   CN10650653

▎ 摘  要

NOVELTY - Porous film comprises 10-40 pts. wt. silicone rubber precursor, 0.05-2 pts. wt. graphene, 50-90 pts. wt. solvent, and 0.5-40 pts. wt. non-solvent or pore-forming agent. USE - Porous film used as artificial skin or surgical dressings for covering mammalian skin-defective wound from bacterial infection (claimed). ADVANTAGE - The porous film has simple preparation technique, controllable thickness, excellent antibacterial activity, and promotes healing. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing porous film, which involves: (A) mixing silicone rubber precursor, graphene, non-solvent or porogen and solvent under stirring mechanically at room temperature to obtain film forming liquid; (B) standing obtained film forming liquid or degassing under vacuum, putting into mold to form a embryo film with thickness of 100 mu m to 3mm; (C) placing obtained embryo film under the environment of 25-60 degrees C for 2-60 minutes and then placing at 100-150 degrees C; and (D) removing non-solvent or porogen from obtained film to obtain final film with a pore size of 500-150 mu m.