▎ 摘 要
NOVELTY - Performing green synthesis of reduced graphene oxide involves mixing a quantity of carbon source in an acid under stirring to obtain solution. The obtained solution is added with a first oxidant to oxidize the carbon source and obtain a suspension. The suspension is stirred at 35 degrees C, and then added with Nigella sativa seed extract under stirring at 60 degrees C. The obtained suspension is added with hydrogen peroxide. The resulting reduced graphene oxide nanoparticles are isolated by centrifugation. USE - Method for performing green synthesis of reduced graphene oxide (claimed).