▎ 摘 要
NOVELTY - Method for preparing a conductive asphalt mixture involves (a) mixing 10-15 wt.% phenol, 8-15 wt.% formaldehyde, 25-30 wt.% 3,4-ethylenedioxythiophene, 5-10 wt.% dicumyl peroxide, 5-10 wt.% reduced graphene oxide, 3-10 wt.% glass fiber, 2-8 wt.% silicon nitride and remaining of water, and stirring, heating at 80-95 degrees C, reacting for 4-10 hours, and keeping warm to obtain wear-resistant conductive material, (b) adding bitumen and aromatic oil to the wear-resistant conductive material mixture, raising the temperature to 165-175 degrees C and stirring for 30-60 minutes, and (c) firstly swelling the mixed material after stirring, keeping the temperature constant during the swelling process, shear testing and developing the mixed material to obtain the conductive asphalt mixture. USE - The method is used for preparing a conductive asphalt mixture (claimed). ADVANTAGE - The method produces an asphalt mixture with high conductivity, high strength and toughness, hydrophobicity, oxidation resistance, and wear resistance.