• 专利标题:   Anticorrosive paint useful in ships comprises epoxy resin, modified basalt flake/carbon nitride composite material, samarium and copper co-doped zinc oxide/graphene composite material, filler, auxiliary agent and water.
  • 专利号:   CN114032003-A, CN114032003-B
  • 发明人:   LI S, HUO X, ZHANG M, GUO X, FENG Y, LIU P
  • 专利权人:   QINGDAO ADVANCED MARINE MATERIAL TECHNOL
  • 国际专利分类:   C09D163/00, C09D005/08, C09D007/61, C09D007/62
  • 专利详细信息:   CN114032003-A 11 Feb 2022 C09D-163/00 202241 Chinese
  • 申请详细信息:   CN114032003-A CN11290855 02 Nov 2021
  • 优先权号:   CN11290855

▎ 摘  要

NOVELTY - Anticorrosive paint comprises 40-60 pts. wt. epoxy resin, 5-15 pts. wt. modified basalt flake/carbon nitride composite material, 3-8 pts. wt. samarium and copper co-doped zinc oxide/graphene composite material, 10-18 pts. wt. filler, 1.5-6 pts. wt. auxiliary agent and 20-30 pts. wt. water. USE - The anticorrosive paint is useful for ships (claimed). ADVANTAGE - The paint: has excellent adhesive force, wear resistance and antibacterial effect; can realize high and low temperature and high salinity performance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the anticorrosive paint comprising firstly placing epoxy resin, modified basalt flake/carbon nitride composite material, samarium and copper co-doped zinc oxide/graphene composite material and water into a high-speed stirrer to mixing, stirring at the speed of 3000-4000 rotation/minute (rpm) for 20-40 minutes, then adding the filler and auxiliary agent into the mixture and continuing stirring for 20-40 minutes to obtain the final product.