• 专利标题:   Preparation of coated stainless steel mesh film involves cleaning stainless steel mesh film, chemical etching, chemical modifying, soaking in graphene oxide-silica coating liquid, washing with deionized water, drying, sintering and cooling.
  • 专利号:   CN104888496-A, CN104888496-B
  • 发明人:   DU H, LI P, LIU J, LV X, HE W, XIA S
  • 专利权人:   UNIV JIANGSU
  • 国际专利分类:   B01D017/022, C02F001/40
  • 专利详细信息:   CN104888496-A 09 Sep 2015 B01D-017/022 201581 Pages: 10 Chinese
  • 申请详细信息:   CN104888496-A CN10222708 04 May 2015
  • 优先权号:   CN10222708

▎ 摘  要

NOVELTY - Preparation of coated stainless steel mesh film comprises cleaning stainless steel mesh film, chemical etching, chemical modifying, soaking in graphene oxide-silica coating liquid, washing with deionized water, chemical modifying, soaking and chemical modifying repeatedly, drying, sintering at 500-550 degrees C for 3-4 hours in the presence of nitrogen and cooling. USE - Method for preparing coated stainless steel mesh film. ADVANTAGE - The coated stainless steel mesh film has strong corrosion resistance, high oil-water separation effect and Escherichia coli inhibitory effect, and has long service life. The method is simple and environment-friendly, and has low production cost.