• 专利标题:   Preparation of graphene oxide and graphene hollow fiber comprises putting outer layer and inner layer solutions in coaxial needles, injecting outer layer to receiving solution, drying, and reducing.
  • 专利号:   CN103031618-A, CN103031618-B
  • 发明人:   ZHAO Y, QU L, JIANG Z
  • 专利权人:   BEIJING INST TECHNOLOGY
  • 国际专利分类:   D01D005/06, D01D005/24, D01F001/08, D01F009/08
  • 专利详细信息:   CN103031618-A 10 Apr 2013 D01F-009/08 201373 Pages: 11 Chinese
  • 申请详细信息:   CN103031618-A CN10579527 26 Dec 2012
  • 优先权号:   CN10579527

▎ 摘  要

NOVELTY - Preparation of graphene oxide and graphene hollow fiber comprises putting outer layer and inner layer solutions in outer and inner layer coaxial needles, injecting outer layer solution to a receiving solution, and drying to obtain graphene oxide hollow fiber; and reducing to obtain graphene hollow fiber. The outer layer solution is 20-25 mg/ml luteinizing graphene oxide. The inner layer solution and receiving solution are greater than or equal to 3 mol/L methanol solution of potassium chloride. The inner layer solution flow rate is 6 ml/minute. The outer layer solution flow rate is greater than or equal to 0.1 ml/second. USE - Method for preparing graphene oxide and graphene hollow fiber (claimed). ADVANTAGE - The method is simple, low cost, and has no need for post-process and impurity removal.