• 专利标题:   Production of lithium ion battery graphene-modified carbon anode material by mixing petroleum asphalt, coal asphalt or mesophase asphalt and graphene, conducting oxidation reaction, mixing with lithium battery solvent and spray drying.
  • 专利号:   CN104445146-A, CN104445146-B
  • 发明人:   SHAN B, CAI F, HAN T, WANG L, YE T, WANG M
  • 专利权人:   DALIAN HONGGUANG LITHIUM CO LTD
  • 国际专利分类:   C01B031/02, H01M004/587
  • 专利详细信息:   CN104445146-A 25 Mar 2015 C01B-031/02 201535 Pages: 6 Chinese
  • 申请详细信息:   CN104445146-A CN10666062 20 Nov 2014
  • 优先权号:   CN10666062

▎ 摘  要

NOVELTY - Production of lithium ion battery graphene-modified carbon anode material comprises providing petroleum asphalt, coal asphalt or mesophase asphalt as raw material A, taking modifier i.e. graphene as raw material B, mixing raw materials A and B, obtaining material C, subjecting material C to oxidation reaction, obtaining material D, taking lithium battery solvent as raw material E, mixing materials D and E, spray drying, conducting graphitization treatment to obtain graphitized material, sieving and packaging to obtain the product. USE - Production of lithium ion battery graphene-modified carbon anode material. ADVANTAGE - The lithium ion battery graphene-modified carbon anode material has good low temperature performance and stable circulation performance. DETAILED DESCRIPTION - Production of lithium ion battery graphene-modified carbon anode material comprises providing petroleum asphalt, coal asphalt or mesophase asphalt as raw material A having particle size distribution (D50) of 50-600 nm, taking modifier i.e. graphene as raw material B having D50 of 5-100 nm, mixing raw materials A and B at 80-95/5-20 weight ratio for 2-5 hours, obtaining material C, subjecting material C to oxidation reaction at 200-260 degrees C for 3-5 hours, obtaining material D, taking lithium battery solvent as raw material E, mixing materials D and E at 30-50/60-100 volume ratio by stirring for 1-5 hours, spray drying at 500-1300 degrees C, conducting graphitization treatment at 2400-3200 degrees C to obtain graphitized material, sieving and packaging to obtain the product.