▎ 摘 要
NOVELTY - Weaving process for home textile product with antibacterial and temperature regulation functions involves obtaining the warp yarn by blending phase change material fiber, long-staple cotton fiber and graphene acrylic fiber, where the dry weight ratio of the phase change material fiber, the long-staple cotton fiber and the graphene acrylic fiber in the warp yarn is 1:(3-5):(0.8-1.2), and the warp density is 120-140 strands/10 cm, preparing the phase change material fiber from a phase change material and polyester fiber, the weft yarn comprises combed cotton blended yarn, silver fiber, bamboo charcoal fiber and/or milk protein fiber blended, and the weft density is 160-180 roots/10 cm, the weaving process of the home textile product involves winding, warping, pre-weaving, weaving and grey fabric post-processing, in the winding treatment process, using a winding machine to make warp yarns and weft yarns into twisted packages. USE - Weaving process used for home textile product with antibacterial and temperature regulation functions. ADVANTAGE - The home textile product prepared by the process is soft, skin-friendly, comfortable, antibacterial and health care, is not easy to pilling, has excellent moisture absorption, air permeability and temperature regulation functions. DETAILED DESCRIPTION - Weaving process for home textile product with antibacterial and temperature regulation functions involves obtaining the warp yarn by blending phase change material fiber, long-staple cotton fiber and graphene acrylic fiber, where the dry weight ratio of the phase change material fiber, the long-staple cotton fiber and the graphene acrylic fiber in the warp yarn is 1:(3-5):(0.8-1.2), and the warp density is 120-140 strands/10 cm, preparing the phase change material fiber from a phase change material and polyester fiber, the weft yarn comprises combed cotton blended yarn, silver fiber, bamboo charcoal fiber and/or milk protein fiber blended, the dry weight ratio of combed cotton blended yarn, silver fiber, bamboo charcoal fiber and milk protein fiber in the weft yarn is 1:(0.2-0.4):(0.1-0.3):(0.1-0.3), and the weft density is 160-180 roots/10 cm, the weaving process of the home textile product involves winding, warping, pre-weaving, and weaving and grey fabric post-processing, in the winding treatment process, using a winding machine to make warp yarns and weft yarns into twisted packages, and the speed of the grooved package is 350 plus minus 5 rpm during winding, the weaving process adopts a JAT-710 type loom, the loom speed is 230-350 rpm, the warp yarn tension is 50-80 CN, and the weft yarn tension is 120-160 CN.