NOVELTY - Reducing graphene oxide antistatic-titanium dioxide (TiO2) composite photocatalytic material preparation comprises preparing reducing graphene oxide solution, heating titanium liquid at 70-95 degrees C, dropping to heating graphene oxide solution for 15-30 minutes, boiling for 50-70 minutes, stirring for 20-40 minutes, heating to boil, adding dilution water to initial reaction volume, filtering solid, washing until neutral, drying solid, roasting for 2-5 hours at 350-450 degrees C, cooling solid in dry bottle, reducing graphene oxide to obtain TiO2 composite photocatalytic material. USE - Method of reducing graphene oxide antistatic-titanium dioxide (TiO2) composite photocatalytic material preparation (claimed).