▎ 摘 要
NOVELTY - A corrosion-resistant composition comprises 100 pts. wt. polyetheretherketone resin, 0.5-10 pts. wt. graphene oxide, 1-10 pts. wt. surfactant, and 100-500 pts. wt. water. USE - Corrosion-resistant composition is used for forming coating (claimed). ADVANTAGE - The corrosion-resistant composition has excellent strength, adhesiveness, and thermal conductivity (provided by graphene oxide). The components are stably and uniformly dispersed.