NOVELTY - The high-temperature-resistant antibacterial non-woven fabric is prepared by: performing alkali decrement treatment on the grey cloth of the non-woven fabric to obtain a pre-treated non-woven fabric; padding the pretreated non-woven fabric into the preliminary finishing liquid for 40-80 minutes, taking out the non-woven fabric, and drying to obtain the preliminary finished non-woven fabric; padding the preliminarily finished non-woven fabric into the after-finishing liquid for 30-60 minutes to obtain the after-finished non-woven fabric; and drying and shaping the post-finished non-woven fabric to obtain a high-temperature-resistant antibacterial non-woven fabric. The preliminary finishing liquid comprises 3-6 pts. wt. chitosan, 2-4 pts. wt. palygorskite powder, 3-5 pts. wt. nano titanium dioxide, 0.8-1.5 pts. wt. Houttuynia cordata extract, 0.5-1 pts. wt. licorice extract; 1-2 pts. wt. a dispersant and 90-120 pts. wt. deionized water. USE - High-temperature-resistant antibacterial non-woven fabric. ADVANTAGE - The non-woven fabrics has improved antibacterial property and strength under high temperature.