▎ 摘 要
NOVELTY - A graphene mortar comprises 15-20 pts. wt., preferably 17 pts. wt. acrylate emulsion, 5-20 pts. wt., preferably 9 pts. wt. cement, 25-40 pts. wt., preferably 28 pts. wt. fine sand, 1-5 pts. wt., preferably 3 pts. wt. water reducer, 6-12 pts. wt., preferably 8 pts. wt. fly ash, 1-8 pts. wt., preferably 5 pts. wt. aluminum slag, 2-7 pts. wt., preferably 4 pts. wt. graphene, 40-50 pts. wt., preferably 45 pts. wt. water, 1-5 pts. wt., preferably 3 pts. wt. antifreeze, and 3-7 pts. wt., preferably 5 pts. wt. defoamer. The water is industrial pure water. USE - Graphene mortar. ADVANTAGE - The graphene mortar has excellent performance, leakage resistance, and high strength, and is prepared using simple and easy method. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the graphene mortar.