▎ 摘 要
NOVELTY - The method for preparing modified graphene, involves preparing reaction mixture composed of 1 part mass graphite oxide, 1-2 parts mass diphenyl disulfide and 1-2 parts mass diphenyl selenide, and heating at 900-1200 degrees C for 2 hours under argon gas protection. USE - Method for preparing modified graphene. ADVANTAGE - The method enables preparation of modified graphene with high surface activity and catalytic activity.