▎ 摘 要
NOVELTY - Graphene material composite glass comprises 46.7-50 wt.% silicon oxide (SiO2), 30-30.3 wt.% calcium carbonate (CaCO3), 10-13.3 wt.% sodium carnonate (Na2CO3), 6.7-10 wt.% boric acid, and the balance is made up of inevitable impurities. USE - Graphene material composite glass. ADVANTAGE - The graphene material composite glass has good antibacterial properties, avoids various air microorganisms from adhering to the glass, has a killing effect on various bacteria and viruses, and because graphene is added inside, and enhanced the thermal conductivity of the composite glass, and easy to use for a long time. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a graphene material composite glass, which involves: (A) adding 5-7 pts. wt. of quartz sand to the container, carrying out acid leaching, and continue to stirring, after acid leaching for five minutes, filter, washing various times and drying; (B) crushing 3-5 pts. wt. limestone and collecting the limestone powder; (C) adding quartz sand and limestone to the container, adding 1-2 pts. wt. of soda ash, adding 100 ml of saturated sodium chloride solution, stirring for a period of time, filtering and drying; (D) adding the mixed powder to the crucible, adding 1 pts. wt. of boric acid, putting the crucible in the crucible box, sealing the crucible box, and then drying the air inside; (E) passing argon gas at 2 times atmospheric pressure for calcination; (F) completing the calcination, then slowly lower the temperature after the glass liquid is formed; (G) cooling down to 1000 degrees C, then quickly adding 0.8 pts. wt. graphene powder through the external interface of the crucible box, stirring, and slowly cooling down; and (H) dropping temperature to 500 degrees C, open the crucible box, taking out the crucible, pouring the glass liquid into the glass mold, and then cooling.