• 专利标题:   Manufacture of positive electrode sheet for lithium-ion battery, involves coating slurry containing positive electrode active material on current collector coated with mixture containing conductive graphene, baking and rolling.
  • 专利号:   CN104518200-A, CN104518200-B
  • 发明人:   CHEN J, LV H, ZHOU W, YIN Y
  • 专利权人:   WANXIANG EV CO LTD, WANXIANG GROUP CO, ZHEJIANG WANXIANG YINENG POWER BATTERY, WANXIANG 123 STOCK CO, WANXIANG EV CO LTD, WANXIANG GROUP CORP
  • 国际专利分类:   H01M004/139, H01M004/62
  • 专利详细信息:   CN104518200-A 15 Apr 2015 H01M-004/139 201554 Pages: 10 Chinese
  • 申请详细信息:   CN104518200-A CN10459260 30 Sep 2013
  • 优先权号:   CN10459260

▎ 摘  要

NOVELTY - Manufacture of positive electrode sheet involves mixing binder, graphene powder, N-methylpyrrolidone and solvent, stirring, obtaining conductive graphene paste having solid content of 10-18%, coating resultant paste on current collector, obtaining coated current collector, mixing binder, N-methylpyrrolidone, conductive agent and positive electrode active material, coating resultant slurry on coated current collector, baking resultant product at 90-120 degrees C for 8-12 hours, obtaining semi-finished product, and rolling resultant material. USE - Manufacture of positive electrode sheet used for lithium-ion battery. ADVANTAGE - The lithium-ion battery provided with the positive electrode sheet has excellent durability, and reduced internal resistance and cell polarization. DETAILED DESCRIPTION - Manufacture of positive electrode sheet involves mixing binder, graphene powder, N-methylpyrrolidone and solvent, stirring, obtaining conductive graphene paste having solid content of 10-18%, coating resultant paste on current collector, obtaining coated current collector, mixing binder, N-methylpyrrolidone, conductive agent and positive electrode active material, coating resultant slurry on coated current collector, baking resultant product at 90-120 degrees C for 8-12 hours, obtaining semi-finished product, and rolling resultant material. The mass ratio of binder and graphene powder is 1.5-7:1.