• 专利标题:   Preparation of antimicrobial air purification membrane involves dissolving specified polymers in organic solvent, obtaining polymers spinning solution, adding graphene oxide, and electrospinning side by side in spinning device.
  • 专利号:   CN103774345-A, CN103774345-B
  • 发明人:   LI J, REN Y, TIAN E, ZHOU H, WANG X
  • 专利权人:   CHINESE ACAD SCI CHONGQING GREEN INTEL
  • 国际专利分类:   B01D039/00, B01D046/54, D04H001/4382, D04H001/728
  • 专利详细信息:   CN103774345-A 07 May 2014 D04H-001/4382 201444 Pages: 7 Chinese
  • 申请详细信息:   CN103774345-A CN10034394 24 Jan 2014
  • 优先权号:   CN10034394

▎ 摘  要

NOVELTY - Preparation of antimicrobial air purification membrane involves dissolving polymers (A) and (B) in organic solvent, obtaining polymer (A) and polymer (B) spinning solution, adding graphene oxide to the obtained spinning solution, obtaining stable uniform polymer (A)-graphene oxide spinning solution and polymer (B)-graphene oxide spinning solution, adding the resultant spinning solutions into a spinning syringe, placing in a spinning device, electrospinning side by side, simultaneously moving the needle back and forth, and obtaining air purification membrane. USE - Preparation of antimicrobial air purification membrane (claimed). ADVANTAGE - The method enables preparation of antimicrobial air purification membrane having excellent filtration efficiency and inhibitory rate of 90%. DETAILED DESCRIPTION - Preparation of antimicrobial air purification membrane involves selecting polymer (A) obtained by electrospinning of crude fiber having diameter of 60-150 nm, and polymer (B) obtained by electrospinning of fine fiber having diameter of 50-350 nm, dissolving the polymers (A) and (B) in organic solvent, obtaining polymer (A) and polymer (B) spinning solution, adding graphene oxide to the obtained spinning solution, obtaining stable uniform polymer (A)-graphene oxide spinning solution and polymer (B)-graphene oxide spinning solution, adding the resultant spinning solutions into a spinning syringe, placing in a spinning device, electrospinning side by side, simultaneously moving the needle back and forth, and obtaining air purification membrane having thickness of 5-200 mu m. The mass ratio of polymer (A) and polymer (B) is 0.5:1-20:1. The mass ratio of polymer (A) and graphene oxide is 10:1-1000:1. The mass ratio of polymer (B) and graphene oxide is 50:1-700:1.