▎ 摘 要
NOVELTY - Double-curing architectural coating comprises 40-50 pts. wt. melamine resin oligomer, 5-50 pts. wt. photo-curing monomer, 0.05-2.5 pts. wt. photoinitiator and 0.5-5 pts. wt. photothermal material. The photo-thermal material comprises at least one of Mxene, graphene and/or ferroferric oxide. USE - The double-curing architectural coating is useful for decorating a building or protecting the building coating. ADVANTAGE - The double-curing architectural coating: has improved curing efficiency; forms a double-network interpenetrating system with high mechanical strength; and reduces the heat energy consumption thus gets rid of the dependence on the environment. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for using method of double-curing architectural coating, comprising applying the double-curing architectural coating to the target building and curing for 4-6 hours under the environment of light intensity of 100-300lx.