• 专利标题:   Polypropylene-based thermoplastic cable shielding material comprises ethylene propylene block copolymer polypropylene, conductive carbon black, highly conductive graphene, coupling agent and additive comprising antioxidant and lubricant.
  • 专利号:   CN112280231-A
  • 发明人:   HOU S, FU M, LI X, HUI B, ZHU W, XUE Z, XU M, CHEN J, HUANG H, GU L, ZHANG Y, FENG B
  • 专利权人:   CSG ELECTRIC POWER RES INST CO LTD, GUANGZHOU POWER SUPPLY BUREAU
  • 国际专利分类:   C08K013/02, C08K003/04, C08K005/098, C08K005/20, C08L053/00, C08L083/04
  • 专利详细信息:   CN112280231-A 29 Jan 2021 C08L-053/00 202118 Pages: 9 Chinese
  • 申请详细信息:   CN112280231-A CN11099806 14 Oct 2020
  • 优先权号:   CN11099806

▎ 摘  要

NOVELTY - Polypropylene-based thermoplastic cable shielding material comprises 100 pts. wt. ethylene propylene block copolymer polypropylene, 3-20 pts. wt. conductive carbon black, 0.5-1.5 pts. wt. highly conductive graphene, 0.5-1.5 pts. wt. coupling agent and 1.4-4.5 pts. wt. additive, where the additive comprises antioxidant, lubricant and anti-caking agent, and the amount of ethylene segments in the ethylene-propylene block copolymer polypropylene is 5-30 %mass. USE - As polypropylene-based thermoplastic cable shielding material. ADVANTAGE - The polypropylene-based thermoplastic cable shielding material improves conductivity, reduces mechanical performance, and has excellent electrical conductivity and mechanical property under high temperature conditions. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing the polypropylene-based thermoplastic cable shielding material, which involves (i) uniformly mixing the conductive carbon black, the highly conductive graphene and the coupling agent to obtain a conductive mixture, (ii) melt blending the ethylene-propylene block copolymer polypropylene, conductive mixture, antioxidant, lubricant and anti-caking agent at 180-210 degrees C, performing water-cooled pelletizing, drying and dehydrating to obtain a polypropylene-based thermoplastic, and (iii) heat-treating the polypropylene-based thermoplastic material obtained in step (ii) at 120-140 degrees C for 2-6 hours to obtain the polypropylene-based thermoplastic cable shielding material.