• 专利标题:   Environmentally-friendly geogrid contains casein, bisphenol A diglycidyl ether, graphene oxide, p-hydroxybenzoic acid, acetic anhydride, zinc acetate, 6-hydroxy-2-naphthoic acid, bisphenol A phosphite, and high-density polyethylene.
  • 专利号:   CN106117729-A
  • 发明人:   YE L
  • 专利权人:   ANHUI GEOMARK SYNTHETIC MATERIAL TECHNOL
  • 国际专利分类:   C08G063/06, C08K013/06, C08K003/04, C08K005/098, C08K005/526, C08K009/04, C08L023/06, C08L025/06, C08L067/04, C08L083/04, C08L091/06
  • 专利详细信息:   CN106117729-A 16 Nov 2016 C08L-023/06 201718 Pages: 5 Chinese
  • 申请详细信息:   CN106117729-A CN10500697 30 Jun 2016
  • 优先权号:   CN10500697

▎ 摘  要

NOVELTY - An environmentally-friendly geogrid contains casein, bisphenol A diglycidyl ether, graphene oxide, p-hydroxybenzoic acid, acetic anhydride, zinc acetate, 6-hydroxy-2-naphthoic acid, bisphenol A phosphite, high-density polyethylene, ammonium molybdate, beeswax, calcium palmitate, polydimethylsiloxane, diisopropyl ethanolamine, sodium diacetate, and polystyrene. USE - Environmentally-friendly geogrid (claimed). ADVANTAGE - The geogrid is safe and environmentally-friendly. DETAILED DESCRIPTION - An environmentally-friendly geogrid contains 1-2 pts. wt. casein, 0.3-1 pts. wt. bisphenol A diglycidyl ether, 5-7 pts. wt. graphene oxide, 40-50 pts. wt. p-hydroxybenzoic acid, 10-17 pts. wt. acetic anhydride, 0.08-0.1 pt. wt. zinc acetate, 20-30 pts. wt. 6-hydroxy-2-naphthoic acid, 5-7 pts. wt. bisphenol A phosphite, 180-200 pts. wt. high-density polyethylene, 0.6-1 pts. wt. ammonium molybdate, 3-4 pts. wt. beeswax, 1-2 pts. wt. calcium palmitate, 0.1-0.2 pt. wt. polydimethylsiloxane, 0.3-1 pts. wt. diisopropyl ethanolamine, 0.7-1 pts. wt. sodium diacetate, and 2-3 pts. wt. polystyrene. An INDEPENDENT CLAIM is included for preparation of environmentally-friendly geogrid, which involves adding sodium diacetate and calcium palmitate to deionized water, uniformly mixing, stirring the mixture at 60-70 degrees C, adding graphene oxide, acetic anhydride and p-hydroxybenzoic acid to the mixture and then heat preserving for 10-15 minutes, adding sulfuric acid to the mixture and then mixing, adding 6-hydroxy-2-naphthoic acid to the mixture and then stirring at 120-130 degrees C, adding polystyrene and acetylated monomer to the mixture and then stirring, adding anhydrous ethanol and bisphenol A diglycidyl ether to the mixture and then uniformly stirring, adding ammonium molybdate to the mixture and then preheating for 6-10 minutes, adding remaining raw materials to the mixture and then uniformly stirring, placing the mixture in an extruder and then melting, and stretching.