▎ 摘 要
NOVELTY - Modifying titanium dioxide with reduced graphene oxide, comprises mixing titanium dioxide powder with reduced graphene oxide powder in a solution of 1-butanol, and homogenizing the solution using ultrasound and drying at 100 degrees C for 24 hours. The molar ratio of titanium dioxide to 1-butanol is 1:20, and the weight ratio of the reduced graphene oxide to titanium dioxide is 0.1-0.5%. The titanium dioxide is used with a developed surface area of 300 m2/g and a particle size of 400 nm. USE - The process is useful for modifying titanium dioxide with reduced graphene oxide.