▎ 摘 要
NOVELTY - Modified thermal composite material comprises 1-4 pts. wt. graphene, 86-124 pts. wt. acrylonitrile butadiene styrene, 24-38 pts. wt. zinc acrylate resin, 54-76 pts. wt. polylactic acid, 46-62 pts. wt. dimeric sodium phosphate, 12-16 pts. wt. chloropropylstyrene, 10-14 pts. wt. maleic anhydride grafted polypropylene, 8-12 pts. wt. carboxymethyl cellulose sodium, 4-6 pts. wt. Kevlar (RTM: Para-aramid synthetic fiber) fiber , 3-5 pts. wt. polybutylene terephthalate fiber, 1-6 pts. wt. surfactant, 0.4-0.8 pts. wt. conditioning agent and 0.3-0.5 pts. wt. generating agent. USE - The modified thermal composite material is useful in three-dimensional printing notebook computer shell. ADVANTAGE - The modified thermal composite material is environmentally friendly, has radiating property and tensile strength. DETAILED DESCRIPTION - Modified thermal composite material comprises 1-4 pts. wt. graphene, 86-124 pts. wt. acrylonitrile butadiene styrene, 24-38 pts. wt. zinc acrylate resin, 54- 76 pts. wt. polylactic acid, 46-62 pts. wt. dimeric sodium phosphate, 12-16 pts. wt. chloropropylstyrene, 10-14 pts. wt. maleic anhydride grafted polypropylene, 8-12 pts. wt. carboxymethyl cellulose sodium, 4-6 pts. wt. Kevlar (RTM: Para-aramid synthetic fiber) fiber, 3-5 pts. wt. polybutylene terephthalate fiber, 1-6 pts. wt. surfactant, 0.4-0.8 pts. wt. conditioning agent, 0.3-0.5 pts. wt. generating agent, 0.4-0.8 pts. wt. crosslinking agent, 0.7-1.3 pts. wt. compatibilizer, 0.5-1 pts. wt. bridging agent, 0.3-0.5 pts. wt. catalyst, 0.5-0.8 pts. wt. plasticizer, 0.3-0.5 pts. wt. dispersant, 0.4-0.7 pts. wt. tackifier, 1-2.3 pts. wt. curing agent, 0.3-0.5 pts. wt. antioxidant, 0.2-0.4 pts. wt. stabilizer, 1.2-1.8 pts. wt. anti-aging agent and 1.8-2.4 pts. wt. flame retardant.