▎ 摘 要
NOVELTY - A thermally conductive coating comprises a main agent and a curing agent in mass ratio of 2:1-4:1. The main agent comprises 5-35 %mass, preferably 10-25 %mass graphene, 10-60 %mass, preferably 25-45 %mass silicone epoxy resin, 3-10 %mass, preferably 5-7 %mass dispersant/surfactant, 4-40 %mass, preferably 10-30 %mass defoamer and 5-20 %mass, preferably 9-15 %mass solvent, with respect to 100 %mass total content of the main agent. USE - Thermally conductive coating. ADVANTAGE - The high-solid thermally conductive coating has excellent antistatic property, and heat dissipation property and heat resistance due to presence of silicone epoxy resin and graphene as cooling medium.