• 专利标题:   Anti-corrosive rubber material useful for coating printing rubber roller, contains isothiazolinone, zinc oxide, graphene oxide, N-hydroxysuccinimide, 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride and potassium persulfate.
  • 专利号:   CN106188665-A
  • 发明人:   ZHOU Z
  • 专利权人:   TONGLING HONGZHENG NETWORK TECHNOLOGY CO
  • 国际专利分类:   C08K013/06, C08K003/04, C08K005/098, C08K005/47, C08K007/00, C08K007/06, C08K009/02, C08K009/04, C08L025/06, C08L007/00
  • 专利详细信息:   CN106188665-A 07 Dec 2016 C08L-007/00 201721 Pages: 5 Chinese
  • 申请详细信息:   CN106188665-A CN10585544 25 Jul 2016
  • 优先权号:   CN10585544

▎ 摘  要

NOVELTY - An anti-corrosive rubber material comprises isothiazolinone, zinc oxide, graphene oxide, N-hydroxysuccinimide, 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride, tris(nonylphenyl)phosphite, p-aminobenzenesulfonic acid, styrene, potassium persulfate, lanthanum chloride, EDTA, carbon fiber, 20-25% aqueous ammonia, natural rubber, 2-mercaptobenzimidazole, ultra-fine barium sulfate, potassium citrate, calcium propionate, isopropanol, trimethylhydroxyethylethylenediamine and sulfur. USE - Anticorrosive rubber material is useful for coating printing rubber roller. ADVANTAGE - The rubber material has improved corrosion resistance. DETAILED DESCRIPTION - An anti-corrosive rubber material comprises 1-2 pts. wt. isothiazolinone, 1-2 pts. wt. zinc oxide, 10-14 pts. wt. graphene oxide, 6-7 pts. wt. N-hydroxysuccinimide, 10-12 pts. wt. 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride, 1-2 pts. wt. tris(nonylphenyl)phosphite, 7-9 pts. wt. p-aminobenzenesulfonic acid, 30-40 pts. wt. styrene, 0.1-0.2 pt. wt. potassium persulfate, 0.3-0.4 pt. wt. lanthanum chloride, 2-3 pts. wt. EDTA, 1.7-2 pts. wt. carbon fiber, 50-67 pts. wt. 20-25% aqueous ammonia, 100-130 pts. wt. natural rubber, 1-2 pts. wt. 2-mercaptobenzimidazole, 10-12 pts. wt. ultra-fine barium sulfate, 1-2 pts. wt. potassium citrate, 3-4 pts. wt. calcium propionate, 2-3 pts. wt. isopropanol, 0.6-1 pt. wt. trimethylhydroxyethylethylenediamine and 0.8-1 pt. wt. sulfur. An INDEPENDENT CLAIM is included for preparation method of anti-corrosive rubber material.