▎ 摘 要
NOVELTY - A permeable brick comprises 30-33 pts. wt. waste aerated concrete particles, 25-26 pts. wt. red soil, 18-20 pts. wt. quicklime, 7-9 pts. wt. cement, 17-19 pts. wt. sugar filter mud, 9-11 pts. wt. sepiolite, 4-6 pts. wt. silicone oil, 0.7-0.8 pt. wt. sodium silicate, 2.1-2.3 pts. wt. graphene, 0.4-0.6 pt. wt. nano-titanium dioxide, 2.2-2.5 pts. wt. rhodium trioxide, 5-7 pts. wt. hexadecyltrimethoxysilane, 6-8 pts. wt. pomegranate peel, 1-2 pts. wt. sandalwood, 2-3 pts. wt. Cyrtomium fortunei and appropriate amount of water. USE - Self-cleaning high water retention rate permeable brick (claimed). ADVANTAGE - The brick has strong adsorption, high water retention rate, high strength, excellent permeability and effectively purifies the pollutants in sewage, promotes waste utilization as resource, improves product added value, and saves a lot of natural gravel resources. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for manufacture of permeable brick.