▎ 摘 要
NOVELTY - Graphene-based metal abrasion repairing material comprises 5-10 gram graphene, 30-150 gram serpentine powder, 20-40 gram molybdenum powder, 15-55 gram rare earth powder, 90-210 gram copper powder, 35-95 gram nickel powder and 1000-2000 milliliter of 100 normal base oil. USE - Graphene-based metal abrasion repairing material. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing graphene-based metal abrasion repairing material which involves: (A) adding the serpentine powder into the plastic vessel, using 80-90 degrees C hot water to wash, stirring with a wood, pouring out the impurities and water, putting in the ventilation and naturally evaporating the water; (B) adding the serpentine powder, molybdenum powder, rare earth powder, copper powder and nickel powder into drying device to dry at 110-130 degrees C for 100-130 minutes until the water content is less than or equal to 2%; (C) adding the powder into the homogenizer to stir at 2000-3000 revolutions/minute, then adding base oil and continuously stirring for 1-10 hours to obtain the colloid mixture; and (D) putting the colloidal mixture into ultrasonic wave dispersing apparatus for dispersing to obtain the graphene-based metal abrasion repairing material.