▎ 摘 要
NOVELTY - A graphene conductive coating comprises 50-70 pts. wt. basal body resin, 0.5-1.5 pts. wt. dispersant, 20-40 pts. wt. solvent, 0.5-5.0 pts. wt. of 10-25 wt.% graphene solution, 0.5-1.0 pt. wt. photoinitiator and 0.5-1.0 pt. wt. leveling agent. USE - Graphene conductive coating. ADVANTAGE - The coating has excellent dispersibility and film properties. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of graphene conductive coating comprising taking photoinitiator and solvent, dissolving, taking remaining raw materials, mixing at rate of 1000-1500 revolutions/minute (rpm) for 20-30 minutes, adding prepared raw material, stirring at rate of 1500 rpm for 30 minutes, and filtering into 200 mesh.