▎ 摘 要
NOVELTY - Preparing graphene mayan blue material involves adding mayan blue into water at 78-91 degrees C, incubating to obtain slurry, adding graphene into slurry, and mixing to obtain graphene mayan blue slurry mixture. The graphene mayan blue slurry mixture is added at 850-960 degrees C under the protection of inert gas, and kept for 3-10 minutes to obtain graphene mayan blue material. USE - Method for preparing graphene mayan blue material (claimed). ADVANTAGE - The method enables to prepare graphene mayan blue material is more stable and more durable catalytic effect.