• 专利标题:   Mortar comprises cement, shale ash, boron slag, water, porous magnesium oxide fiber, sodium laurate polyoxyethylene ether sulfate, graphene oxide fiber-doped metal ion, and carbon nanotube fibers.
  • 专利号:   CN110436842-A
  • 发明人:   LIANG J
  • 专利权人:   LIANG J
  • 国际专利分类:   C04B111/20, C04B111/27, C04B111/34, C04B028/02
  • 专利详细信息:   CN110436842-A 12 Nov 2019 C04B-028/02 201990 Pages: 11 Chinese
  • 申请详细信息:   CN110436842-A CN10789785 26 Aug 2019
  • 优先权号:   CN10789785

▎ 摘  要

NOVELTY - Mortar comprises 50-60 pts. wt. cement, 30-50 pts. wt. shale ash, 10-20 pts. wt. boron slag, 30-50 pts. wt. water, 3-5 pts. wt. porous magnesium oxide fiber, 0.5-1.5 pts. wt. sodium laurate polyoxyethylene ether sulfate, 1-3 pts. wt. allyl-2-acetamido-2-deoxy-beta-D-glucopyranoside/glyphosic acid C/tributylvinyltin/vinyltrimethoxysilane copolymer, 3-8 pts. wt. graphene oxide fiber-doped metal ion, and 1-3 pts. wt. carbon nanotube fibers. USE - Used as the mortar containing cement. ADVANTAGE - The mortar: has electromagnetic shielding function, wide electromagnetic shielding band, high toughness, crack resistance, good impermeability, high corrosion resistance, and has high compressive strength; and can meet the requirements of different building materials. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the mortar comprising mixing cement, shale ash, boron slag, porous magnesium oxide fiber, sodium laurate polyoxyethylene ether sulfate, allyl-2-acetamido-2-deoxy-beta-D-glucopyranoside/glyphosic acid C/tributylvinyltin/vinyltrimethoxysilane copolymer, graphene oxide fiber-doped metal ion, and carbon nanotube fiber, then adding water, stirring at 60-80 degrees C for 3-5 hours, and cooling to room temperature.