▎ 摘 要
NOVELTY - Current transformer magnetic material comprises 5-9 pts. wt. graphene, 15-18 pts. wt. epoxy resin, 3-7 pts. wt. iron oxide, 9-12 pts. wt. modified clay, 10-15 pts. wt. polyacrylate resin, 2-5 pts. wt. lubricant, 5-8 pts. wt. glycerin, 3-6 pts. wt. poly-aryl ether nitrile, 2-4 pts. wt. manganese oxide, 1-5 pts. wt. cobalt oxide and 6-9 pts. wt. carbonated material. The carbonated material comprises 7-10 pts. wt. calcium carbonate, 4-9 pts. wt. barium carbonate and 2-5 pts. wt. strontium carbonate. USE - Current transformer magnetic material. ADVANTAGE - The material has strong elasticity, stretchability and good high temperature resistance, enhances magnetic property, saves energy and is easy non-demagnetizing and environment friendly.