▎ 摘 要
NOVELTY - Preparation of activated carbon/graphene composite material comprises mixing 45-90 wt.% biomass, 5-50 wt.% carbon nitrogen compound, and 5-10 wt.% transition metal-containing compound, heating to 300-500 degrees C for 2-5 hours to obtain fluffy bulk material, and heating to 600-900 degrees C for 5-60 minutes under protective gas atmosphere. USE - Method for preparation of activated carbon/graphene composite material (claimed). ADVANTAGE - The method is simple and suitable for large-scale production, and it has easy to obtain raw materials.