▎ 摘 要
NOVELTY - Preparing skid-proof paint comprises (i) mixing hyper-branched polymer and organo-silicone resin in a ratio of 3.5-3.8:80, adding 0.12% coupling agent of the mass of organo-silicone, heating mixture to 150-160 degrees C, stirring at 2000-2500 rotations/minute for 2-3 hours and air-cooling to room temperature; (ii) using sericite powder doped with 0.3-3.5 wt.% aminated graphene oxide; and (iii) adding 100-105 pts. wt. modified silicone resin of step (i), 25-30 pts. wt. filler of step (ii), 1-3 pts. wt. dispersing agent, 0.2-1.5 pts. wt. leveling agent, 0.5-1 pts. wt. defoaming agent, 60-100 pts. wt. toluene, mixing uniformly, stirring at 3000 rotations/minute for 2 hours and grinding for another 40 minutes. USE - The method is useful for preparing skid-proof paint. ADVANTAGE - The skid-proof paint has good coating adhesion, weather resistance, wear resistance and high temperature resistance.