▎ 摘 要
NOVELTY - Rubber material comprises 70-80 pts. wt. epoxidized natural rubber, 20-30 pts. wt. butadiene rubber, 2 pts. wt. sulfur, 0.5 pts. wt. accelerator M (2-mercaptobenzothiazole), 0.3 pts. wt. accelerator DM (2,2'-dithiobis(benzothiazole)), 2 pts. wt. stearic acid, 1 pts. wt. paraffin, 5 pts. wt. zinc oxide, 2 pts. wt. antioxidant D (N-cyclohexylidenehydroxylamine), 30-50 pts. wt. spray carbon black, 10-15 pts. wt. chlorinated paraffin, 20-40 pts. wt. aluminum hydroxide, 3-10 pts. wt. graphene, and 5 pts. wt. motor oil. USE - The rubber material is useful for shoe sole (claimed). ADVANTAGE - The rubber material has flame resistance, abrasion resistance and, oil resistance, antistatic property, good air tightness, low temperature resistance and strong gripping force.