• 专利标题:   Preparing wooden composite material involves collecting a pretreated circular veneer with a circular hole in the center, preparing an activating solution A, an activating solution B, activating solution C and an electroless copper solution.
  • 专利号:   AU2021102654-A4
  • 发明人:   PAN Y, HUANG J, YIN D, GUO Q, ZHAO S, DAI M, WANG H, HU N
  • 专利权人:   UNIV INNER MONGOLIA AGRIC
  • 国际专利分类:   B27K003/00, B27K003/16, B27K003/22, B27K003/26, H05K009/00
  • 专利详细信息:   AU2021102654-A4 08 Jul 2021 B27K-003/22 202176 Pages: 38 English
  • 申请详细信息:   AU2021102654-A4 AU102654 18 May 2021
  • 优先权号:   AU102654

▎ 摘  要

NOVELTY - Preparing wooden composite material involves collecting a pretreated circular veneer with a circular hole in the center and with a diameter of 11 cm, preparing an activating solution A, an activating solution B, an activating solution C, an electroless copper solution, an electroless nickel solution, hollow fibers and graphene oxide grafted iron oxide, first placing the circular veneer in the activating solution A for activation, and then placing the circular veneer in the activating solution B for activation, placing the circular veneer treated in the electroless copper solution, adding the hollow fibers, and conducting the electroless copper, first placing the circular veneer treated in the activating solution C for activation, and then placing the circular veneer in the activating solution B for activation. USE - Method for preparing wooden composite material. ADVANTAGE - The method enables to prepare wooden composite material with improved magnetic loss, conductivity loss and interface polarization magnetic relaxation loss. DETAILED DESCRIPTION - Preparing wooden composite material involves collecting a pretreated circular veneer with a circular hole in the center and with a diameter of 11 cm, preparing an activating solution A, an activating solution B, an activating solution C, an electroless copper solution, an electroless nickel solution, hollow fibers and graphene oxide grafted iron oxide, first placing the circular veneer in the activating solution A for activation, and then placing the circular veneer in the activating solution B for activation, placing the circular veneer treated in the electroless copper solution, adding the hollow fibers, and conducting the electroless copper, first placing the circular veneer treated in the activating solution C for activation, and then placing the circular veneer in the activating solution B for activation, placing the circular veneer treated in the step in the electroless nickel solution, adding graphene oxide grafted iron oxide, conducting the electroless nickel operation, and drying to obtain the composite materials.