▎ 摘 要
NOVELTY - Stirrer head modified graphene reinforced nickel-based alloy powder comprises 1-8 wt.% vanadium, 0.1-1 wt.% strontium, 0.1-3 wt.% indium, 3-8 wt.% aluminum, 3-8 wt.% titanium, 1-5 wt.% cobalt, 1-5 wt.% molybdenum, 0.01-0.5 wt.% boron, 0.05-0.5 wt.% erbium, 0.5-5 wt.% graphene, and balance nickel. USE - Stirrer head modified graphene reinforced nickel-based alloy powder. ADVANTAGE - The powder has high efficiency and low production costs.